Al 2 O 3 DENGAN METODA ELEKTROPORETIK

1 DEPOSISI LAPISAN TIPIS KERAMIK KOMPOSIT YSZ/Al 2 O 3 DENGAN METODA ELEKTROPORETIK Kemas A. Zaini Thosin Pusat Penelitian Fisika, LIPI, Gedung 442, K...