PENGARUH PERLAKUAN PANAS TERHADAP KONDUKTIVITAS DAN ENERGI AKTIVASI KOMPOSIT (LiI) x (Al 2 O 3 ) 1-x

1 ISSN Pengaruh Perlakuan Panas Terhadap Konduktivitas dan Energi Aktivasi Komposit (Lil) x(al 2O 3) 1-x (P. Purwanta, S. Purnama, D.S Winatapura, Y. ...