Keywords: GTAW, Fracture Propagation, Stress Corrosion Cracking, Inhibitor Precipation

1 KARAKTERISASI PERILAKU PERAMBATAN RETAK FATIK DAN KOROSI RETAK TEGANG DALAM LARUTAN CaCl 2 40% DENGAN INHIBITOR SODIUM SILIKAT dan ZEOLIT PADA SAMBU...